Most garage "MIG welders" can do two related processes. Gas MIG (GMAW) uses solid wire and a shielding gas from a cylinder. Self-shielded flux-core (FCAW-S) uses tubular wire with flux inside that makes its own shielding, so there's no gas. Both run on the same kind of machine, but they suit different work. Here's how to choose, and which welders in our database do which.
The short answer
- Choose flux-core if you'll weld outdoors, mostly on steel 1/8 in. and thicker, want the lowest startup cost, or don't want to manage a gas cylinder.
- Choose gas MIG if you'll weld indoors, do a lot of thin sheet (auto body, light gauge), and want clean beads with little cleanup.
- Can't decide? Buy a machine that does both. Nearly every gas-capable welder here also runs flux-core, and you can add gas later.
How each process shields the weld
Molten steel reacts with oxygen and nitrogen in the air, which causes porosity (holes) and weak welds. Both processes protect the puddle, but in different ways.
Gas MIG: shielding gas flows out of the nozzle around the wire. For mild steel, the common choices are 75% argon / 25% CO2 (often called C25), which gives a smoother arc and less spatter, or 100% CO2, which is cheaper and penetrates more but spatters more. Aluminum needs 100% argon and usually a spool gun. Stainless typically uses a tri-mix gas.
Self-shielded flux-core: flux inside the wire burns to make shielding gas and a protective slag over the bead. Nothing comes out of a cylinder, so a breeze won't blow the shielding away the way it does with gas MIG.
There's also dual-shield (gas-shielded) flux-core, which uses both flux-cored wire and gas. It's mostly an industrial process for thick steel, and most entry-level machines aren't set up for it.
Side-by-side comparison
| Self-shielded flux-core | Gas MIG (solid wire) | |
|---|---|---|
| Gas cylinder | None | Required (buy or lease from a welding gas supplier) |
| Outdoors / wind | Tolerates a breeze | Shielding blows away; needs still air or wind screens |
| Appearance | Slag to chip and brush off; more spatter | Clean bead, little spatter |
| Thin sheet (under ~18 ga.) | Harder; burns through more easily | Easier to control |
| Dirty or rusty steel | More forgiving (still clean it) | Needs clean, bare metal |
| Smoke and fumes | More | Less, but still requires ventilation |
| Typical polarity | DCEN (electrode negative) | DCEP (electrode positive) |
| Running cost | Wire costs more per pound | Cheaper wire, plus gas refills |
Polarity matters. Switching between flux-core and solid wire usually means moving the gun and ground leads inside the machine. Your manual shows how.
Wire basics
The most common self-shielded flux-core wire for home machines is E71T-GS. The "GS" means it's intended for single-pass welds, so it isn't meant for building up thick joints with many passes. E71T-11 wires allow multiple passes within the maker's thickness limits. Read the wire maker's data sheet.
The standard solid wire for gas MIG on mild steel is ER70S-6, which has extra deoxidizers that help on slightly dirty steel. Sizes .023–.030 in. suit thin sheet, and .030–.035 in. suit general garage work. Match the drive roll to the wire: knurled for flux-core, smooth V-groove for solid wire. See welding wire.
What gas actually adds to the cost
For gas MIG you need a regulator/flowmeter (many machines include one), a hose, and a cylinder. Small cylinders can be bought outright or leased from local welding gas suppliers, and refills are swaps at the counter. Prices vary a lot by region, so call a couple of local suppliers before you buy. Secure the cylinder upright with a chain or strap, keep the valve cap on when it isn't connected, and open the valve slowly while standing to the side. See regulators.
Which machines do which
Flux-core only (no gas valve or solenoid): Lincoln Electric WELD-PAK 90i FC (K5255-1), Forney Easy Weld 141 FC-i (262), YesWelder FLUX-135PRO and ARCCAPTAIN MIG135. All are on the flux-core page.
Gas MIG + flux-core: Lincoln Electric WELD-PAK 90i MIG (K5256-1), Everlast Cyclone 140E, Everlast Cyclone 200ES, PrimeWeld MIG180 and Miller Millermatic 142 (907838). See gas MIG welders.
Multi-process (MIG, flux-core, stick, lift-TIG): most of the dual-voltage machines in our database. See multi-process welders.
| Welder | Type | Input | MIG output | Steel (maker) | Approx. price | Shop |
|---|---|---|---|---|---|---|
| Flux-core only | 120V | 20–120 A | 18 ga. to 1/4 in. | $300–$500 | Amazon ↗ | |
| Gas MIG + flux-core | 120V | 20–120 A | 24 ga. to 1/4 in. (flux-cored); 3/16 in. (MIG) | $300–$500 | Amazon ↗ | |
| Flux-core only | 120V | Up to 140 A | 24 ga. to 1/4 in. | $200–$300 | Amazon ↗ | |
| Gas MIG + flux-core | 120V | 25–140 A | Up to 3/16 in. single pass; 3/8 in. multi-pass (min. 24 ga.) | $300–$500 | Amazon ↗ |
Safety differences
Flux-core makes noticeably more smoke. Both processes produce fumes you shouldn't breathe, so weld with the garage door open and a fan pulling fumes away from you (not blowing across the gas-MIG arc), or use fume extraction. Wear a respirator in tight spaces. Never weld galvanized, painted or plated steel without grinding the coating off first. Zinc fumes from galvanizing can cause metal fume fever. Both processes throw sparks and spatter, so clear flammables and keep an extinguisher close. See the welding safety gear guide.
Welding can cause electric shock, burns, eye injury, fire and exposure to hazardous fumes. Read your welder's manual before use, wear proper PPE, and ventilate. Have a licensed electrician install or check any 240V outlet or circuit. This site gives general information only, not professional or electrical advice. Safety basics →